PROPERTY |
TEST METHOD |
RESULT TYPICAL |
|
Tensile Strength Elongation |
ASTM D-638 Type I ASTM D-638 Type I? |
707 psi (49.7 kg/cm sqr) 19.4% |
|
Compressive Strength Modulus |
ASTM D-695 |
2264 psi (159.2 kg/cm sqr) 4660 psi (327.6 kg/cm sqr) |
|
Impact Strength |
ASTM D-256 "A" |
1.46 ft. lbs./in. (0.079 kg m/cm) |
|
Bond Strength |
ASTM D-1002 (modified 0.5 in./min.) Tensile Lap Shear |
1051 psi (73.9 kg/cm sqr) |
|
Hardness determined by PPG |
ASTM 2240 Shore D |
25 after 24 hrs. at 20°C |
|
Density |
Practical density after spraying |
68.7 lbs./ft. cubed (1.1 g/cc) |
|
Thermal Conductivity |
ASTM C-177 K. Value |
1.69 BTU In./°F ft. sqr hr. (0.244 W/m °C) |